Product Description:
1. PB-09 Burnishing Skim Coat is a two-component, high-strength, cement-based mortar with fine-grained selected aggregates, special admixtures and synthetic polymers in water dispersion.
2. When the two components (component A powder and component B liquid) are mixed together, an easy-spread mix is obtained which may be applied manually on vertical surfaces at a thickness of up to 2 mm per layer.
Features and Benefits:
1. Crackless application.
2. Mixes easily with potable water.
3. High-ductility smoothing and leveling layer on concrete repaired.
4. High bonding strength
5. Impermeable to water and aggressive gases present in the atmosphere
Operation Process:
1, Using spatula to scraping mixed polishing lacquer putty onto the surface (requiring one or two times).
2, After 8h using sand paper for polishing.
Tips:
a, Using appropriate scraper to scrap the lacquer putty on the surface.
b, Mixing the PB-09 with water into paste, electric mixer can get better effect. put it aside for a few minutes and then a little stirring to strengthen the hardness.
Dosage:
1~1.2kg/m² /mm of thickness, depending on thickness and condition of base coat.
Few dosages for the even surface
Store Method:
Store in cool and dry place, unopened product can be saved for one year.
Technical Reference:
Coverage area(amount) |
Technical reference |
About 1.8~2.5kg/,according to the smoothness of the surface
|
1, status: powder, evenly without caking |
2,operation: no scratching barrier |
|
3, dry time: under 4h |
|
4, water resistance(48h): normal |
|
5, alkaline resistance(24h): normal |
|
6, shear strength under standard pressure: 1.2MPa |
|
7, shear strength after water resistance: 0.9MPa |
|